Stir contents before using.
FIRST COAT
Apply the plaster with a flexible steel trowel, apply a thin coat of plaster while holding the trowel at a 15- to
30-degree angle. Spread the plaster with varying lengths and angles of strokes. Clean off the trowel from
time to time to keep dried plaster from getting into your burnish. Let the plaster dry thoroughly before
applying the next coat.
SECOND COAT
Apply thin layer of plaster, use overlapping long and short strokes. Cover the surface thoroughly, filling voids
and removing high spots. Let the plaster dry for at least 24 hours before moving on to the burnish treatment.
Apply VELLWAX and buff off evenly will add durability to the surface.
COVERAGE / THINNING
Five kilogram (11 Lbs) covers up 60 – 80 sq. ft. on a smooth wall, significantly less on acoustical tile or rough
surface. We do not recommend thinning down the plaster but if you wish to create other effect, thinning not
more than 1 oz. (29.6ml mL) of water per 11 Lbs (5 kg) of plaster.
Five kilogram (55 Lbs) covers up 300 – 400 sq. ft. on a smooth wall, significantly less on acoustical tile or
rough surface. We do not recommend thinning down the plaster but if you wish to create other effect,
thinning not more than 5 oz. (148ml) of water per 55 Lbs (25 kg) of plaster.
DRYING TIME
Plaster only when surface and air temperatures are 50-90 °F (10-32 °C), wait 24 hours before recoating or
applying MACOAVELL VELLWAX.